Which type of test covers the fracture acceptable after a 180° bend?

✓

Direct Answer

Option A: Bend tests

Bend tests of welded joints verify ductility and root soundness, requiring that no fracture or crack develops after undergoing a standard 180° guided bend.

All Options

A
Bend tests (Correct Answer)
B
Charpy V-notch impact tests
C
All of the above
D
Tensile tests

Detailed Explanation & Context

Bend tests of welded joints verify ductility and root soundness, requiring that no fracture or crack develops after undergoing a standard 180° guided bend.

Relevant Framework: STCW 2010 Manila Amendments • DG Shipping E-Learning & Exit Exam Standards • Advanced Training for Ships subject to the IGF Code (AIGF).

Advertisement

Practice Full AIGF Set 2

Test yourself with 30 interactive questions, live timer, and instant score.

Launch Practice Simulator →

Question Discussion & Notes

0

Have a doubt, memory trick, or exam update? Share your insights with fellow mariners.

Leave a Comment / Clarification

By posting, you agree to our Terms & Moderation Policy.

Loading mariner discussions...