Pyrophoric oxidation occurs when loading:

✓

Direct Answer

Option D: Chemical cargoes

Pyrophoric iron sulphide oxidation occurs when pyrophoric scale (formed by hydrogen sulphide reacting with rust in low-oxygen conditions) is exposed to oxygen when loading or ventilating tanks.

All Options

A
Light crude oils
B
Sour crude oils
C
Refined products
D
Chemical cargoes (Correct Answer)

Detailed Explanation & Context

Pyrophoric iron sulphide oxidation occurs when pyrophoric scale (formed by hydrogen sulphide reacting with rust in low-oxygen conditions) is exposed to oxygen when loading or ventilating tanks.

Relevant Framework: STCW 2010 Manila Amendments • DG Shipping E-Learning & Exit Exam Standards • Oil and Chemical Tanker Cargo Operations (OCTCO/OCTF).

Advertisement

Practice Full OCTCO/OCTF Set 4

Test yourself with 30 interactive questions, live timer, and instant score.

Launch Practice Simulator →

Question Discussion & Notes

0

Have a doubt, memory trick, or exam update? Share your insights with fellow mariners.

Leave a Comment / Clarification

By posting, you agree to our Terms & Moderation Policy.

Loading mariner discussions...